Contact Us

Size guide · chapter 02

Walls, grades and the only number worth comparing

Two different conversations get mixed together constantly: how a box was built, and what condition it is in now. Construction is the wall and the ECT. Condition is the grade. You need both.

Specify it properly

Tell us wall and grade and the quote arrives without a follow-up

The grade field is optional — if you leave it blank we will recommend one based on what you are putting in the box.

A working address — this is where the quote goes.
US or Canada only — 10 digits, in the shape (614) 000-0000. We format it as you type
Two-letter code or full name (OH or Ohio).
US ZIP (43228 or 43228-1234) or Canadian code (M5V 2T6)
Whole units, at least 1.
Pick a suggestion or describe it.
Pick a suggestion or describe it.
Optional — we will recommend one.

No phone calls — we are an email-first yard. Your details go to our sales desk only, never to a list broker.

Construction

Three wall types, and what each one buys you

A flute is the wavy layer that does the structural work. More layers means more column strength, more weight, more cost and — importantly — more reuse cycles.

2 flutes, 3 liners

Double wall

The default for reusable gaylords. Comfortable to about 1,400 lb, stacks two high, flat-packs easily. Roughly 70% of our stock.

32 – 48 ECT

3 flutes, 4 liners

Triple wall

For 1,800 lb and up, three-high stacking and sharp contents. Heavier and pricier per box, but reuses more times — so cost per trip often lands lower.

51 – 71 ECT

double or triple + barrier

Waxed / coated

Curtain-coated or impregnated wax for hydro-cooled produce, iced loads and outdoor storage. Cannot go into standard recycling, so we take it back separately.

44 – 61 ECT

ECT

Edge Crush Test, in plain language

A one-inch-wide strip of board is stood on its edge and squeezed until it buckles. The force at failure, in pounds per inch, is the ECT. That is the whole test — and it maps almost directly onto how a box behaves at the bottom of a stack.

ECT ratings and what they survive
ECTWallComfortable loadStack heightWhere you see it
32Double800 – 1,100 lb2 highLight scrap, foam, trim
40Double1,200 – 1,400 lb2 highProduce, bakery, general
44Double1,500 – 1,700 lb2 highThe yard workhorse
48Double+1,700 – 1,900 lb2 – 3 highHeavier general warehousing
51Triple2,200 – 2,500 lb3 highMetal parts, regrind
61Triple2,700 – 3,000 lb3 highCastings, cullet, dense bulk
71Triple+3,200 – 3,400 lb3 highMaximum industrial duty
Burst strength is the wrong number hereBurst (Mullen) testing measures puncture resistance, which matters for parcels taking knocks in a sorting centre. Bulk boxes fail by crushing under their own stack, so ECT is the figure to compare. If a supplier quotes you burst strength for a gaylord, ask for ECT instead.

Condition

Our grading sheet, written out in full

We grade by hand against this. It is published so that “used” cannot quietly drift in meaning between your first order and your tenth.

A

Like new

1 trip · $11.80 – $14.20

Clean interior, square rim, all four corners sound, no delamination, no print bleed. Will pass a visual inspection on a food-adjacent line.

✓ Food-adjacent packing✓ Customer-facing shipments✓ Export loads✕ Scrap handling✕ Internal WIP
B

Solid workhorse

2 – 3 trips · $8.20 – $10.90

Scuffs, a taped corner, often a stencil from a previous job. Rim intact, at least three sound corners, stackable two to three high. The grade most buyers should be ordering.

✓ General warehousing✓ Returns processing✓ Most manufacturing✕ Food contact without a liner
C

One more trip

4 – 5 trips · $6.40 – $7.90

Soft top edge, a patched panel, honest visible wear. Structurally fine for a single additional run with dry goods. Stack two high at most.

✓ Internal WIP bins✓ Scrap and trim✓ Dry goods, short moves✕ Three-high stacking✕ Anything shipped to a customer
R

Recycle grade

end of life · market OCC rate

Delaminated, mouldy or crushed beyond use. Sold baled as OCC commodity, never as boxes. We would rather tell you this than sell you a bad grade C.

✓ Baling and repulping✕ Any load-carrying use

Inside the board

Flute profiles, and why C-flute runs this industry

The wavy middle layer does the structural work. Its height and frequency decide crush resistance, cushioning and how well the board prints — and bulk boxes have settled almost entirely on C and its double and triple combinations.

FluteHeightFlutes per footCharacterWhere you meet it
A3/16" (4.8 mm)33 ± 3Highest stacking, best cushioningRare in bulk boxes; fragile goods
B1/8" (3.2 mm)47 ± 3Good crush resistance, poor cushioningInner layer of double wall; canned goods
C11/64" (4.0 mm)39 ± 3The all-round compromiseDominant flute in gaylords and shipping cases
E1/16" (1.6 mm)90 ± 4Low stacking, excellent print surfaceRetail cartons; never a bulk box
BC1/4" (6.4 mm)double wallStrong, the common double wallMost used gaylords on our floor
AC / ACA3/8"+ (9.5 mm+)triple wallMaximum column strength61 – 71 ECT bulk bins, castings, cullet
Used flat-packed corrugated stacked on pallets inside an older brick warehouse

The check that comes before every other check

Moisture is the only failure we cannot grade around

Corrugated board exchanges moisture with the air until it reaches equilibrium. At 50% relative humidity it performs to spec; at 85% it has lost roughly a quarter of its compression strength, and once liquid water has broken the liner-to-flute bond the loss is permanent.

That is why a grader’s hand goes on the panel before anything else, and why a box that looks perfect can still be recycle grade.

Derating

What humidity does to a rated load

Humidity damage is reversible; liquid water damage is not. The practical distinction a grader makes is whether the panel still sounds tight when pressed.

Relative humidityBoard moistureCompression strengthWhat we would do
30%5.5%108% of ratedStronger than spec — board is dry
50%7.0%100% of ratedLaboratory reference condition
65%9.0%88% of ratedAcceptable; watch the trend
80%11.5%74% of ratedMove the stack or add airflow
90%14.0%62% of ratedStop storing board here entirely

Condition in the field

What a well-stored lot looks like

Flat corrugated board stored on edge in a galvanised A-frame rack
Stored properlyVertical racking keeps board off the slab and square. Four inches of air on every side, oldest at the front.
The four-inch ruleOn a pallet, never on the slab. Four inches of air on every side. No stretch wrap in storage. Away from dock doors and exterior walls. Oldest at the front. That single paragraph covers 90% of the board we have to bale.

Grading questions

The things people ask once they understand grading

Who decides the grade — you or me?

We do, by hand, and then we show you photographs of the actual pallet. If you disagree before it ships, we re-price. If you disagree after it arrives, we collect it and refund the freight.

Can I mix grades on one order?

Yes, and many customers should. Grade B for anything leaving the building, grade C for internal bins. We palletise them separately and label them.

Does grade affect how many more trips I get?

Yes, roughly. Grade A has five to seven trips left, grade B three to five, grade C one to two. BoxPrint projects exactly this for any reference you type in.

Why is there no grade D?

Because it would be a lie. Below grade C the honest answer is recycle grade, and we sell that by the bale at commodity rates.

Reference · 01

Every defect we grade against

Published so a downgrade is never a matter of opinion, and so your receiving team can speak the same language.

DefectWhat it looks likeCauseGrade effectRepairable?
DelaminationLiner lifts away from the flutes; the panel sounds hollowLiquid water, or sustained humidity above 85%Recycle grade, alwaysNone
Rim crushTop edge flattened or folded overOverloaded stack, or no lidUnder 2" → B; soft all round → C; torn → recycleNone economic
Corner failureVertical corner split, bulged or tapedPoint loading or a dropped unit loadThree sound → B; two sound + repair → CTape and corner board
Fork punctureRound hole 2–4" above the deckTine entering a flat stack at the wrong heightBelow the load line → CPatch and hot-melt
Dragged cornerLower corner folded and abradedMast carried too low; habitual at a siteB → CRarely repairable
Out of squareBox leans; opposite rim corner lifts when pressedRe-folded off the original score linesUnder 0.5" → B; under 1" → CNone
Joint separationManufacturer's seam openingFatigue, or an over-filled boxRecycle gradeNone economic
Flute crushPanel feels thin, flat crush resistance goneOver-tight strapping, or a crushed pallet stackC at bestNone
MouldSpotting, musty smellWet board held wrapped for daysRecycle grade, automaticNone — never resold
ResiduePowder, oil or food matter insidePrevious contentsJudged separately from conditionReject or route to non-food use

Reference · 02

Standards and test methods

What the box maker's certificate certifies against, and which number is worth comparing.

ReferenceMethodMeasuresWhy it matters here
TAPPI T 811Edge crush test (ECT)Force to buckle a 1-inch board edge, lb/inPredicts stacking strength — the number that matters for bulk boxes
TAPPI T 810Burst (Mullen) testPressure to rupture the board, psiPuncture resistance; relevant to parcels, not gaylords
TAPPI T 804Box compression test (BCT)Force to crush a whole box, lbThe direct measure; destructive, so rarely run on used stock
TAPPI T 839Flat crushFlute resistance, psiDetects crushed flutes from over-tight converting
ASTM D4169Distribution cycle testingSimulated transit damageWhat a customer's packaging engineer asks about
ISTA 3BPackaged-product testing, LTLDrop, vibration, compressionOccasionally specified for bulk shipments
Rule 41 / Item 222Carrier classification rulesMinimum board for a given size and gross weightWhat the box maker's certificate is certifying against
ISO 12048Compression and stackingStatic load enduranceUsed in export specifications
ISPM 15Wood packaging treatmentHeat treatment of palletsPallets crossing borders, not the corrugated

Next step

Not sure which grade your load needs?

Describe what is going in the box. We have talked plenty of customers down a grade and saved them a third of their packaging spend.